Rod Anode for Cooler VOLVO PENTA serie 200-250-270

serie - 200-250-270
PART NO. | 00713 | 00713T complete | 00713TP plug only |
Weight | 0.060kg/0.13lbs | 0.100kg/0.22lbs | 0.040kg/0.09lbs |
l | 67mm/2.64” | ||
a | 13mm/0.51” | 13mm/0.51” | |
b | 10mm/0.39” | 10mm/0.39” | |
c | 40mm/1.57” | 40mm/1.57” | |
Ø | 15mm/0.59” | 15mm/0.59” | |
Ø1 | 1/2”BSPT | 1/2”BSPT | |
Ø2 | 7/16”unc |